Product Copper Tube

Type of Copper

KS D 5301 Properties and Uses Related Standards
Alloy No. Shape Rank Sign JIS ASTM BS DIN KS
C1201 TUBE Nomal C1201T
  • The properties for enduring the pressure, bending, drawing, welding, corrosion, thermal, conductivity are excellent.
  • C1201 does not create hydrogen embrittlement when it is heated in the high temperature reduction environment.
  • C1201 is better then C1220 in electric conductivity
  • For heat exchanger, chemical industry, water supply, rapid boiling and gas pipes.
H3300
C1201
C1220
B88
C12010
C12200
2871
C106
1789
SW-Cu
SF-Cu
D5301
C1201
C1220
Special C1201TS
C1220 TUBE Nomal C1220T
Special C1220TS

Chemical Commposition and Characteristic

Elements Alloy No Chemical composition(%)
Cu P
Phosporus
Deoxidized Copper
C1201 99.90 min 0.004 min ~ 0.015 max
C1220 99.90 min 0.015 min ~ 0.040 max
Specific Gravity Melting-temperature(°C) Specific heat(Cal/g°C) Coefficient of thermal expansion
20°C 100°C -191~16°C 20~100°C 20~200°C
8.94 1,083 0.0921 0.0939 14.1×10-6 16.8×10-6 17.3×10-6
Conductivity
(Kcal/mhr°C)
Electrical conductivity
(IACS%)
Electrical resistance
(㎕ ㎝)
332 100 2.5~1.9

Mechanical Properties (KS D 5301)

Alloy Temper
Designation
Size Mechanical Rockwell Hardness
Outside Diameter(㎜) Thickness(㎜) Tensile Strength(N/㎟) Elongation(%) HR30T HR15T HRF
C1201T
C1220T
0 C1220T-0 4min~250max 0.25min~30max 205min 40min 60max 50max
0L C1220T-0L 4min~250max 0.25min~30max 205min 40min 65max 55max
1/2H C1220T-1/2H 4min~250max 0.25min~30max 245~325 30~60
H C1220T-H 25max 0.25min~30max 55min
25초과~50max 0.9min~4.0max 315min
50초과~100max 1.35min~6.0max
100초과~200max 2.0min~6.0max 275min
200초과~350max 3.0min~6.0max 255min